Hello people: I'm new to carcraft and a "newbie starter" to spraygun painting. Please try not to laugh too hard at me because this is my first post and i'm new to painting.I will create a profile soon, but for now, I have an 05/Ram/1500/Hemi/QC/Red
I'm in the process of colormatching my door handles on my truck. They are the textured plastic. I sanded all the texture off, washed them very well, &wax&grease remover. Before priming, I used bulldog ad promoter and within 10 minutes I was spraying a nason urathane primer(nason 2k 421-19). After 24hrs of dry time, I had seen there was 2 huge blisters on the flat part of the handle assembly. With the exception of those two blisters, the primer adhered very well. Any thoughts?
Many thanks Don
Also, I have had my psi(at the gun) set to 42(stupid me). Is that too much? I recently found this out that it should be no more than about 23-25.
Rollin On 4:56's
|
|
Posted: 05/21/08 04:21 PM
|
|
Do you have a picture of the blisters? that can help a ton. I know its an old post now but still...
|
|
|